Optical constants of OHARA - BAM (Barium, medium-index)
BAM25
Wavelength:
µm
(0.360 – 0.9)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.513482-0.008739639λ^{2}+0.0186819λ^{-2}+0.0007470892λ^{-4}-3.047596\text{×}10^{-05}λ^{-6}+3.39904\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.6357e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.603230 Vd: 42.320943 glass_code: 603423 glass_status: preferred density: 3.46 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.4e-06 K-1 - temperature_range: 20 300 ℃ coefficient: 9.5e-06 K-1
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets