Optical constants of OHARA - BAM (Barium, medium-index)
BAM12
Wavelength:
µm
(0.365 – 0.9)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.628582-0.009085873λ^{2}+0.0195519λ^{-2}+0.0006698928λ^{-4}-2.510153\text{×}10^{-05}λ^{-6}+3.047777\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.9903e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.639300 Vd: 44.878032 glass_code: 639449 glass_status: preferred density: 3.8 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.6e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.7e-06 K-1 dPgF: -0.0001
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)