Optical constants of OHARA - BAL (Barium, low-index)
L-BAL43
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.04745291λ^2}{λ^2-0.00563209756}+\frac{0.428452873λ^2}{λ^2-0.0188321416}+\frac{1.14111303λ^2}{λ^2-114.197069}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.03e-06 9.62e-09 -1.13e-11 4.9e-07 5.73e-10 0.199 nd: 1.585729 Vd: 59.696980 density: 3.05 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.2e-06 K-1 dPgF: 0.5415 climatic_resistance: 3.0 acid_resistance: 51.4 phosphate_resistance: 2.0
Comments
Low Softening Temperature
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets