Optical constants of OHARA - BAL (Barium, low-index)
L-BAL42
Wavelength:
µm
(0.29 – 0.9)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.39528097λ^2}{λ^2-0.011186203}+\frac{0.072551952λ^2}{λ^2+0.0246748575}+\frac{1.66335848λ^2}{λ^2-167.717958}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.46e-06 9.17e-09 -3.83e-11 4.68e-07 4.9e-10 0.21 nd: 1.583126 Vd: 59.385694 glass_code: 583594 density: 3.05 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.2e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.8e-06 K-1 dPgF: -0.0031 climatic_resistance: 1.0 acid_resistance: 5.2 phosphate_resistance: 2.0
Comments
Low Softening Temperature
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets