Optical constants of OHARA - BAL (Barium, low-index)
L-BAL35P
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.806742194λ^2}{λ^2-0.0148836231}+\frac{0.690488648λ^2}{λ^2-0.00251943058}+\frac{1.26477947λ^2}{λ^2-111.31457}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 5.03e-06 1.22e-08 -3.81e-11 4.93e-07 5.76e-10 0.16 nd: 1.592080 Vd: 60.993997 density: 2.82 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.6e-06 K-1 dPgF: -0.0046 climatic_resistance: 3.0 acid_resistance: 52.2 phosphate_resistance: 3.2
Comments
Low Softening Temperature
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets