$$n^2=2.4686122-0.0099937773λ^{2}+0.013115756λ^{-2}+0.00045052253λ^{-4}-3.1570294\text{×}10^{-05}λ^{-6}+1.7307442\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C nd: 1.583126 Vd: 59.373789 glass_code: 583594 glass_status: preferred