Optical constants of OHARA - BAL (Barium, low-index)
BAL41
Wavelength:
µm
(0.350 – 0.9)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.410742-0.010238λ^{2}+0.01233414λ^{-2}+0.0003782378λ^{-4}-2.550448\text{×}10^{-05}λ^{-6}+1.456385\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 4.4071e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.563839 Vd: 60.695914 glass_code: 564607 glass_status: preferred density: 2.78 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.8e-06 K-1 - temperature_range: 20 300 °C coefficient: 9.1e-06 K-1 dPgF: -0.0029
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets