Optical constants of OHARA - BAH (Barium, high-index)
BAH32
Wavelength:
µm
(0.3 – 2.4)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.498643λ^2}{λ^2-0.009643255}+\frac{0.2175678λ^2}{λ^2-0.04511666}+\frac{1.559728λ^2}{λ^2-171.1121}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 6.7962e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.669979 Vd: 39.279752 glass_code: 670393 glass_status: preferred density: 4.02 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.1e-06 K-1 acid_resistance: 1.2 phosphate_resistance: 1.0
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets