Optical constants of OHARA - BAH (Barium, high-index)
BAH27
Wavelength:
µm
(0.365 – 0.9)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.823151-0.01090859λ^{2}+0.02374898λ^{-2}+0.000901646λ^{-4}-3.713171\text{×}10^{-05}λ^{-6}+5.48189\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 4.1987e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.701536 Vd: 41.242277 glass_code: 702412 glass_status: preferred density: 4.02 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.5e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.5e-06 K-1 dPgF: 0.0024
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets