Optical constants of OHARA - BAH (Barium, high-index)
BAH10
Wavelength:
µm
(0.365 – 0.9)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.730459-0.01063385λ^{2}+0.01942756λ^{-2}+0.0008209873λ^{-4}-5.210457\text{×}10^{-05}λ^{-6}+4.447534\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 25.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.2706e-06 0.0 0.0 0.0 0.0 0.0 nd: 1.670029 Vd: 47.253429 glass_code: 670473 glass_status: preferred density: 3.77 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.1e-06 K-1 - temperature_range: 20 300 °C coefficient: 8.2e-06 K-1 dPgF: -0.0006
References
OHARA Zemax catalog 2017-11-30 (obtained from http://www.ohara-inc.co.jp)
See also OHARA glass data sheets