Optical constants of HIKARI - multiple purpose
NIFS-V
Wavelength:
µm
(0.157 – 2.500)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.640349086λ^2}{λ^2-0.004253794}+\frac{0.374308316λ^2}{λ^2-0.012779842}+\frac{0.089750539λ^2}{λ^2-0.014004437}+\frac{0.908924481λ^2}{λ^2-99.3231891}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 22.5 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.21e-05 3e-08 -1.14e-12 2.52e-07 4.92e-10 0.235 nd: 1.458564 Vd: 67.859016 density: 2.2 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.3e-07 K-1 dPgF: -0.002 climatic_resistance: 1.0 stain_resistance: 0.0 acid_resistance: 1.0 alkali_resistance: 1.0 phosphate_resistance: 1.0
Comments
TCE value is available for 25 to 300 degrees Celsius.
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also NIKON synthetic silica glass data sheet
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon