Optical constants of HIKARI - multiple purpose
NIFS-S
Wavelength:
µm
(0.18489 – 2.500)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.565169763λ^2}{λ^2-0.003823156}+\frac{0.422092787λ^2}{λ^2-0.011444418}+\frac{0.11689465λ^2}{λ^2-0.015169704}+\frac{0.883720207λ^2}{λ^2-96.4254081}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 22.5 °C thermal_dispersion: - type: "Schott formula" coefficients: 2.15e-05 3.84e-08 -5.68e-13 3.33e-07 3.98e-10 0.184 nd: 1.458477 Vd: 67.826411 density: 2.2 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.3e-07 K-1 dPgF: -0.0021 climatic_resistance: 1.0 stain_resistance: 0.0 acid_resistance: 1.0 alkali_resistance: 1.0 phosphate_resistance: 1.0
Comments
TCE value is available for 25 to 300 degrees Celsius.
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also NIKON synthetic silica glass data sheet