Optical constants of HIKARI - multiple purpose
5742
Wavelength:
µm
(0.310 – 2.400)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2-1=\frac{1.30326513λ^2}{λ^2-0.00977713845}+\frac{0.127313632λ^2}{λ^2-0.0463756328}+\frac{0.895143157λ^2}{λ^2-107.962139}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 22.5 °C thermal_dispersion: - type: "Schott formula" coefficients: 4.25e-07 1.13e-08 2.44e-13 9.33e-07 8.92e-10 0.201 nd: 1.576531 Vd: 42.042478 density: 3.15 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.7e-06 K-1 dPgF: -0.0024 climatic_resistance: 1.0 acid_resistance: 2.0 alkali_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also NIKON i-line glass data sheet
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links