$$n^2-1=\frac{1.12790724λ^2}{λ^2-0.00673602593}+\frac{0.129745283λ^2}{λ^2-0.0228274219}+\frac{0.994872985λ^2}{λ^2-94.2587142}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 22.5 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.48e-06 1.89e-08 2.59e-13 3.58e-07 4.09e-10 0.212 nd: 1.511829 Vd: 64.957110 density: 2.44 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 5.8e-06 K-1 dPgF: -0.0044 climatic_resistance: 1.0 acid_resistance: 4.0 alkali_resistance: 1.0