Optical constants of HIKARI - Glasses for precision molding
Q-LASF03S

Wavelength: µm
 (0.320 – 2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=3.1699583-0.012153683λ^{2}-0.000127440597λ^{4}+0.0309253962λ^{-2}+0.000733513997λ^{-4}+6.0190839\text{×}10^{-06}λ^{-6}+2.17380961\text{×}10^{-06}λ^{-8}$$

Conditions & Spec sheet

n_absolute: false
wavelength_vacuum: false
temperature: 23.0 °C
thermal_dispersion:
  - type: "Schott formula"
    coefficients: 1.0303e-05 1.4294e-08 -9.4458e-13 8.9892e-07 1.0565e-09 0.21112
nd: 1.806040
Vd: 40.737356
density: 4.48 g/cm3
thermal_expansion:
  - temperature_range: -30 70 °C
    coefficient: 7.1e-06 K-1
dPgF: -0.007
phosphate_resistance: 3.0

Comments

For mold lens

References

NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

INFO

Hikari Glass Co., Ltd.

Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.