Optical constants of HIKARI - Glasses for precision molding
Q-FKH2S
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.10025148-0.00458689757λ^{2}-2.09903123\text{×}10^{-05}λ^{4}+0.00685727645λ^{-2}+2.32345667\text{×}10^{-05}λ^{-4}+4.89859472\text{×}10^{-06}λ^{-6}-1.82336191\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -1.998e-05 -7.2484e-09 -1.0199e-12 3.9343e-07 3.3572e-10 0.10375 nd: 1.455620 Vd: 91.307727 density: 3.67 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.34e-05 K-1 dPgF: 0.0431 phosphate_resistance: 4.0
Comments
For mold lens
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data