Optical constants of HIKARI - SSK (Very dense crown)
J-SSK5
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.69546608-0.00946960473λ^{2}-0.000110686762λ^{4}+0.0190535266λ^{-2}+0.000349767067λ^{-4}+1.61235917\text{×}10^{-06}λ^{-6}+1.06076791\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: -4.0838e-07 1.2283e-08 -2.4387e-12 5.7044e-07 5.5102e-10 0.21181 nd: 1.658440 Vd: 50.835655 density: 3.75 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7e-06 K-1 dPgF: -0.0013 phosphate_resistance: 3.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon