Optical constants of HIKARI - SSK (Very dense crown)
E-SSK8
Wavelength:
µm
(0.340 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.57047824-0.0119686463λ^{2}+0.0149712411λ^{-2}+0.00112845548λ^{-4}-0.000110413826λ^{-6}+7.39815032\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.617720 Vd: 49.779142 glass_status: preferred density: 3.22 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.4e-06 K-1 dPgF: -0.0008
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links