Optical constants of HIKARI - SSK (Very dense crown)
E-SSK1
Wavelength:
µm
(0.4 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.56935287-0.0103280973λ^{2}+0.0161803173λ^{-2}+0.000314456596λ^{-4}-8.91235286\text{×}10^{-08}λ^{-6}+6.08967029\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.617200 Vd: 54.009900 glass_status: preferred density: 3.32 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.9e-06 K-1 dPgF: -0.0016
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon