Optical constants of HIKARI - SK (Dense crown)
SK18
Wavelength:
µm
(0.330 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.652537-0.02070769λ^{2}+0.008235652λ^{-2}+0.0025989λ^{-4}-0.0003027232λ^{-6}+1.591967\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.638540 Vd: 55.479588 glass_code: 639555 glass_status: preferred density: 3.69 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.1e-06 K-1 dPgF: -0.0021
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon