Optical constants of HIKARI - SK (Dense crown)
SK15
Wavelength:
µm
(0.290 – 0.7)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.595129-0.01330175λ^{2}+0.01295053λ^{-2}+0.000946977λ^{-4}-9.281618\text{×}10^{-05}λ^{-6}+5.074742\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.622990 Vd: 58.225167 glass_code: 623582 glass_status: preferred density: 3.66 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.1e-06 K-1 dPgF: -0.0018
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon