Optical constants of HIKARI - SK (Dense crown)
J-SK15
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.59035665-0.0102907579λ^{2}-0.000119847148λ^{4}+0.0157254882λ^{-2}+0.000190519844λ^{-4}+6.52864472\text{×}10^{-06}λ^{-6}-1.78313721\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 1.3614e-06 1.4372e-08 -1.7642e-12 4.6435e-07 4.093e-10 0.17738 nd: 1.622990 Vd: 58.122114 density: 3.58 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6e-06 K-1 dPgF: -0.003 phosphate_resistance: 2.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets