Optical constants of HIKARI - SK (Dense crown)
J-SK12
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.46741191-0.00952788845λ^{2}-0.000102594923λ^{4}+0.0140303006λ^{-2}+0.000169265777λ^{-4}+5.39399652\text{×}10^{-06}λ^{-6}-2.33385875\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.1379e-06 1.4764e-08 -2.5759e-12 4.852e-07 5.9867e-10 0.18104 nd: 1.583130 Vd: 59.419851 density: 3.23 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6e-06 K-1 dPgF: -0.0018 phosphate_resistance: 2.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets