Optical constants of HIKARI - SK (Dense crown)
E-SK5
Wavelength:
µm
(0.290 – 0.7)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=2.48616859-0.00962090414λ^{2}+0.0146866348λ^{-2}-0.000117877135λ^{-4}+4.43876615\text{×}10^{-05}λ^{-6}-2.05228288\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.589130 Vd: 61.162060 glass_code: 589612 glass_status: preferred density: 3.2 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.9e-06 K-1 dPgF: -0.0008
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links