Optical constants of HIKARI - SK (Dense crown)
E-SK14
Wavelength:
µm
(0.290 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.53104523-0.0107742896λ^{2}+0.0140100006λ^{-2}+0.000247886041λ^{-4}-1.0881644\text{×}10^{-06}λ^{-6}+1.03415548\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.603112 Vd: 60.669444 glass_code: 603607 glass_status: preferred density: 3.43 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7e-06 K-1 dPgF: -0.0007
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)