Dispersion formula
$$n^2=2.46638796-0.00865760981λ^{2}+0.0144628215λ^{-2}+7.9427451\text{×}10^{-05}λ^{-4}+1.55773822\text{×}10^{-05}λ^{-6}-5.24586883\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.583130 Vd: 59.387186 glass_status: preferred density: 3.09 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.7e-06 K-1 dPgF: -0.0019