Optical constants of HIKARI - SF (Dense flint)
SFS3
Wavelength:
µm
(0.360 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.071402-0.02168875λ^{2}+0.02943887λ^{-2}+0.005498532λ^{-4}-0.0005380916λ^{-6}+4.131754\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.784700 Vd: 26.207574 glass_code: 785262 glass_status: preferred density: 5.02 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9e-06 K-1 dPgF: 0.0077
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links