Optical constants of HIKARI - SF (Dense flint)
SF8
Wavelength:
µm
(0.340 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.798858-0.03718093λ^{2}+0.007630191λ^{-2}+0.007231691λ^{-4}-0.0008073847λ^{-6}+4.696667\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.688930 Vd: 31.144745 glass_code: 689311 glass_status: preferred density: 4.22 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 9.3e-06 K-1 dPgF: 0.0015
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets