Optical constants of HIKARI - SF (Dense flint)
SF4
Wavelength:
µm
(0.350 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.988119-0.03043514λ^{2}+0.0237723λ^{-2}+0.005097428λ^{-4}-0.0004379463λ^{-6}+3.025835\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.755200 Vd: 27.641217 glass_code: 755276 glass_status: preferred density: 4.79 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.5e-06 K-1 dPgF: 0.0055
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets