Optical constants of HIKARI - SF (Dense flint)
SF14
Wavelength:
µm
(0.380 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.983846-0.01289956λ^{2}+0.03563966λ^{-2}+0.002969076λ^{-4}-0.000222699λ^{-6}+2.674236\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.761820 Vd: 26.556302 glass_code: 762266 glass_status: preferred density: 4.57 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.5e-06 K-1 dPgF: 0.0122
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets