Optical constants of HIKARI - SF (Dense flint)
SF13
Wavelength:
µm
(0.380 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.92263-0.01150018λ^{2}+0.02875835λ^{-2}+0.004472855λ^{-4}-0.0004973006λ^{-6}+4.089372\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.740771 Vd: 27.644962 glass_code: 741276 glass_status: preferred density: 4.37 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.1e-06 K-1 dPgF: 0.0093
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets