Optical constants of HIKARI - SF (Dense flint)
J-SFS3
Wavelength:
µm
(0.370 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.05623339-0.0128486167λ^{2}+0.0387408706λ^{-2}+0.00339109066λ^{-4}-0.000605526065λ^{-6}+0.000141221664λ^{-8}-1.44464234\text{×}10^{-05}λ^{-10}+6.88155857\text{×}10^{-07}λ^{-12}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -4.097e-06 1.0254e-08 -1.1078e-12 9.8475e-07 1.5745e-09 0.28971 nd: 1.784700 Vd: 26.268169 density: 3.28 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.4e-06 K-1 dPgF: 0.0128 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets