Optical constants of HIKARI - SF (Dense flint)
J-SF6HS
Wavelength:
µm
(0.365 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.11993645-0.0126679163λ^{2}+0.0421698355λ^{-2}+0.00304768926λ^{-4}-0.000420720196λ^{-6}+0.000106770582λ^{-8}-1.09382035\text{×}10^{-05}λ^{-10}+5.57077794\text{×}10^{-07}λ^{-12}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -5.46222e-06 9.79277e-09 2.28229e-12 1.05026e-06 1.51597e-09 0.288402 nd: 1.805180 Vd: 25.448348 density: 3.34 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 8.6e-06 K-1 dPgF: 0.014 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon