Optical constants of HIKARI - SF (Dense flint)
J-SF2
Wavelength:
µm
(0.360 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.63768374-0.0104781511λ^{2}+0.0239749005λ^{-2}+0.00192856512λ^{-4}-0.000366733662λ^{-6}+7.71499779\text{×}10^{-05}λ^{-8}-7.4649885\text{×}10^{-06}λ^{-10}+3.25251898\text{×}10^{-07}λ^{-12}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: -3.9095e-06 9.4107e-09 -8.6488e-13 8.6526e-07 1.0468e-09 0.264 nd: 1.647690 Vd: 33.723654 density: 2.72 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9e-06 K-1 dPgF: 0.0053 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets