Optical constants of HIKARI - SF (Dense flint)
E-SF2
Wavelength:
µm
(0.360 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.63429594-0.00920840209λ^{2}+0.0274266023λ^{-2}+0.000225441472λ^{-4}+9.97644221\text{×}10^{-05}λ^{-6}+1.76259116\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.647689 Vd: 33.799707 glass_code: 648338 glass_status: preferred density: 2.77 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 8.4e-06 K-1 dPgF: 0.0069
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets