Optical constants of HIKARI - SF (Dense flint)
E-SF14
Wavelength:
µm
(0.370 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.98384614-0.0128995609λ^{2}+0.035639664λ^{-2}+0.00296907641λ^{-4}-0.00022269905λ^{-6}+2.67423649\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.761820 Vd: 26.556301 glass_code: 762266 glass_status: preferred density: 3.16 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.4e-06 K-1 dPgF: 0.0122
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon