Optical constants of HIKARI - SF (Dense flint)
E-SF13
Wavelength:
µm
(0.370 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.92006212-0.0134436038λ^{2}+0.0333556844λ^{-2}+0.00246092959λ^{-4}-0.000160492168λ^{-6}+2.11511846\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.740769 Vd: 27.784828 glass_code: 741278 glass_status: preferred density: 3.13 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.1e-06 K-1 dPgF: 0.0115
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets