Optical constants of HIKARI - SF (Dense flint)
E-SF1
Wavelength:
µm
(0.370 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.84827856-0.0122548479λ^{2}+0.0316736954λ^{-2}+0.00170745362λ^{-4}-7.33008941\text{×}10^{-05}λ^{-6}+1.41012815\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.717362 Vd: 29.522238 glass_code: 717295 glass_status: preferred density: 3.07 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 9.7e-06 K-1 dPgF: 0.0101
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon