Optical constants of HIKARI - SF (Dense flint)
E-SF03
Wavelength:
µm
(0.370 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.25492893-0.0156026034λ^{2}+0.0458228209λ^{-2}+0.0037273634λ^{-4}-0.000238976694λ^{-6}+3.42745142\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.846660 Vd: 23.776466 glass_code: 847238 glass_status: preferred density: 3.53 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.02e-05 K-1 dPgF: 0.0158
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)