Optical constants of HIKARI - PSK (Dense phosphate crown)
E-PSK03
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.53132391-0.00865579054λ^{2}+0.0142829487λ^{-2}-0.000115110582λ^{-4}+4.15511576\text{×}10^{-05}λ^{-6}-1.9869836\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.603001 Vd: 65.460398 glass_code: 603655 glass_status: preferred density: 3.52 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 1.05e-05 K-1 dPgF: 0.0062
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)