Optical constants of HIKARI - PSK (Dense phosphate crown)
E-PSK02
Wavelength:
µm
(0.320 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.57651436-0.00817396399λ^{2}+0.0152706397λ^{-2}-0.000117385023λ^{-4}+4.69952008\text{×}10^{-05}λ^{-6}-2.25968944\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C nd: 1.618000 Vd: 63.372017 glass_code: 618634 glass_status: preferred density: 3.55 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 1.1e-05 K-1 dPgF: 0.0067
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)