Optical constants of HIKARI - PK (Phosphate crown)
PK1
Wavelength:
µm
(0.290 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.23377-0.009387074λ^{2}+0.01057538λ^{-2}-3.481847\text{×}10^{-05}λ^{-4}+2.380097\text{×}10^{-05}λ^{-6}-1.340308\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 ℃ nd: 1.503780 Vd: 66.815093 glass_code: 504668 glass_status: preferred density: 2.46 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.4e-06 K-1 dPgF: -0.0018
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links