Optical constants of HIKARI - PK (Phosphate crown)
J-PKH1
Wavelength:
µm
(0.290 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.27892705-0.00904327622λ^{2}-0.000110679206λ^{4}+0.0101870033λ^{-2}+9.31149884\text{×}10^{-05}λ^{-4}+2.7225654\text{×}10^{-06}λ^{-6}-1.82952398\text{×}10^{-08}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 3.9674e-06 1.6064e-08 -1.5853e-12 3.5592e-07 2.7773e-10 0.19762 nd: 1.518600 Vd: 69.890785 density: 2.6 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 6.3e-06 K-1 dPgF: 0.0047 phosphate_resistance: 3.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets