Optical constants of HIKARI - LaSK (Lanthanum dense crown)
E-LASKH2
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.01740929-0.0150192115λ^{2}+0.0220799937λ^{-2}+0.000476675587λ^{-4}-9.36464002\text{×}10^{-06}λ^{-6}+9.63541852\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.754999 Vd: 52.314919 glass_code: 755523 glass_status: preferred density: 4.29 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7e-06 K-1 dPgF: -0.0091