Optical constants of HIKARI - LaSF (Lanthanum dense flint)
Q-LASFPH2S
Wavelength:
µm
(0.300 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.0430437-0.0130169861λ^{2}-0.000175012562λ^{4}+0.025603733λ^{-2}+0.000448879136λ^{-4}+1.131389\text{×}10^{-05}λ^{-6}+4.69755261\text{×}10^{-07}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 8.850929e-06 1.485241e-08 3.179295e-12 7.356564e-07 8.071775e-10 0.1941267 nd: 1.765437 Vd: 46.751378 density: 4.52 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 5.3e-06 K-1 dPgF: -0.0095 phosphate_resistance: 3.0
Comments
For mold lens
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets