Optical constants of HIKARI - LaSF (Lanthanum dense flint)
P-LASFH18S
Wavelength:
µm
(0.330 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.32566886-0.0131396072λ^{2}+0.0340298328λ^{-2}+0.000803745646λ^{-4}+1.03681091\text{×}10^{-05}λ^{-6}+2.05840857\text{×}10^{-06}λ^{-8}-0.000123587896λ^{4}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ nd: 1.851170 Vd: 40.049954 glass_status: preferred density: 5.27 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 7.3e-06 K-1 dPgF: -0.0072
Comments
Low Tg glass
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)