Optical constants of HIKARI - LaSF (Lanthanum dense flint)
LASFH6
Wavelength:
µm
(0.360 – 0.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.167451-0.02220547λ^{2}+0.02630248λ^{-2}+0.004028856λ^{-4}-0.0004018775λ^{-6}+2.821967\text{×}10^{-05}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 20.0 °C nd: 1.806100 Vd: 33.267264 glass_code: 806333 glass_status: preferred density: 4.62 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7.5e-06 K-1 dPgF: -0.0004
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon