Optical constants of HIKARI - LaSF (Lanthanum dense flint)
J-LASFH21
Wavelength:
µm
(0.360 – 2.400)
Derived optical constants
n
k
logX
logY
eV
Dispersion formula
$$n^2=3.67012303-0.0139442893λ^{2}-0.000136361252λ^{4}+0.0484434485λ^{-2}+0.000950687214λ^{-4}+0.000181807808λ^{-6}-1.62618274\text{×}10^{-05}λ^{-8}+1.33939862\text{×}10^{-06}λ^{-10}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 °C thermal_dispersion: - type: "Schott formula" coefficients: 6.76193e-07 6.83583e-09 2.24584e-12 9.81173e-07 1.29551e-09 0.249631 nd: 1.953750 Vd: 32.334656 density: 5.05 g/cm3 thermal_expansion: - temperature_range: -30 70 °C coefficient: 7e-06 K-1 dPgF: 0.0004 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links