Optical constants of HIKARI - LaSF (Lanthanum dense flint)
J-LASFH2
Wavelength:
µm
(0.330 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.04927657-0.0145487808λ^{2}-0.000168864692λ^{4}+0.0251825857λ^{-2}+0.000522534606λ^{-4}+2.91654231\text{×}10^{-06}λ^{-6}+1.27935733\text{×}10^{-06}λ^{-8}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 4.0284e-06 1.2768e-08 -1.9358e-12 6.7798e-07 6.5574e-10 0.17418 nd: 1.766840 Vd: 46.777867 density: 4.11 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 5.5e-06 K-1 dPgF: -0.0083 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets
Data
INFO
Hikari Glass Co., Ltd.
Hikari Glass Co., Ltd. is a Japanese glass maker, a subsidiary of Nikon Corp.External links
- Hikari Glass Co., Ltd. (in Japanese)
- Nikon