Optical constants of HIKARI - LaSF (Lanthanum dense flint)
J-LASFH17HS
Wavelength:
µm
(0.370 – 2.400)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=3.81071676-0.0163737936λ^{2}+0.0583672875λ^{-2}+0.00412726108λ^{-4}-0.000552229126λ^{-6}+0.000141302816λ^{-8}-1.45517862\text{×}10^{-05}λ^{-10}+7.444268\text{×}10^{-07}λ^{-12}$$Conditions & Spec sheet
n_absolute: false wavelength_vacuum: false temperature: 23.0 ℃ thermal_dispersion: - type: "Schott formula" coefficients: 2.4887e-07 1.1853e-08 2.8854e-12 1.1578e-06 1.587e-09 0.28102 nd: 2.000690 Vd: 25.455728 density: 4.69 g/cm3 thermal_expansion: - temperature_range: -30 70 ℃ coefficient: 6.8e-06 K-1 dPgF: 0.0123 phosphate_resistance: 1.0
References
NIKON Zemax catalog 2017-11 (obtained from http://www.nikon.com)
See also HIKARI glass data sheets